Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000125 ohm-cm | 0.0000125 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Alloy 406 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |