Polymer Property : Electrical Resistivity = 0.00001187 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed
Eagle Brass 510 Phosphor Bronzes 5% A, Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..