Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00001175 ohm-cm | 0.00001175 ohm-cm | |
Lucas-Milhaupt Silvaloy® A50N Flux Coated Rod Brazing Alloy Silvacote A50N Flux Cored is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel t.. |
|||
Electrical Resistivity | 0.00001175 ohm-cm | 0.00001175 ohm-cm | |
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy Silvacote A50N Flux Coated Rod is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nic.. |
|||
Electrical Resistivity | 0.00001175 ohm-cm | 0.00001175 ohm-cm | |
Lucas-Milhaupt Silvacote® A50N Brazing Alloy Silvacote A50N is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silve.. |