Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000107 ohm-cm | 0.0000107 ohm-cm | |
Lucas-Milhaupt Premabraze 616 Silver Based Cadmium Free Filler Metal Applications: Application is found in all types of moderate temperature low pressure systems, and in particular the electronic vacuum tube. Characteristics:Premabraze 616 is a low temperature, sl.. |