Polymer Property : Electrical Resistivity = 0.00000890 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, Annealed
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Electrical Resistivity 0.00000890 ohm-cm
0.00000890 ohm-cm
Annealed
Eagle Brass 511 Phosphor Bronzes 4%, Spring
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..