Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.00000862 ohm-cm | <= 0.00000862 ohm-cm | Calculated from Min 20 %IACS |
Cadi 3 MOLD-MOR™ The hardest and highest strength copper alloy, Beryllium copper is specified when the mechanical strength is the limiting design feature for a copper alloy.Forms: RodBarPlateInformation provided by .. |