Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.00000860 ohm-cm | <= 0.00000860 ohm-cm | |
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Electrical Resistivity | <= 0.00000860 ohm-cm | <= 0.00000860 ohm-cm | |
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Electrical Resistivity | 0.00000860 ohm-cm | 0.00000860 ohm-cm | Castings (20 % IACS) |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |