Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899D 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899D Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899E 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899E Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899L Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899A Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899G 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899G Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Electrical Resistivity | 0.00000763 ohm-cm @Temperature 20.0 °C |
0.00000763 ohm-cm @Temperature 68.0 °F |
|
Ametek High Purity Nickel Strip 899M Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |