Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000555 ohm-cm | 0.00000555 ohm-cm | Calculated from 31 %IACS |
Cadi 100W Tungsten Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |