Polymer Property : Electrical Resistivity = 0.00000410 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000410 ohm-cm
0.00000410 ohm-cm
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se..
Electrical Resistivity 0.00000410 ohm-cm
0.00000410 ohm-cm
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy
This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f..
Electrical Resistivity <= 0.00000410 ohm-cm
<= 0.00000410 ohm-cm
MarkeTech WCu30 Tungsten Copper Alloy
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Electrical Resistivity 0.00000410 ohm-cm
0.00000410 ohm-cm
precipitation hardened (3 hr)
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000410 ohm-cm
0.00000410 ohm-cm
precipitation hardened (2 hr)
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000410 ohm-cm
0.00000410 ohm-cm
(42% IACS)
CMW® ELKONITE® TC10 Tungsten Carbide Copper material
For wiping and arcing electrical contacts and projection welding tips.Information provided by CMW Inc.