Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000390 ohm-cm | 0.00000390 ohm-cm | Conductivity is 44% IACS |
Materion Alloy 390 Beryllium Nickel Strip Alloy 390 was specifically designed for high power applications, providing a unique combination of high strength and high conductivity. Increasing power requirements are driving the need for lower c.. |