Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000350 ohm-cm | 0.00000350 ohm-cm | |
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Electrical Resistivity | 0.00000350 ohm-cm @Temperature 20.0 °C |
0.00000350 ohm-cm @Temperature 68.0 °F |
|
Materion AlBeMet® AM 162 HIP'd Billet, Annealed This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) .. |
|||
Electrical Resistivity | 0.00000350 ohm-cm | 0.00000350 ohm-cm | |
Mi-Tech Metals CW70 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Electrical Resistivity | 0.00000350 ohm-cm @Temperature 20.0 °C |
0.00000350 ohm-cm @Temperature 68.0 °F |
|
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Electrical Resistivity | 0.00000350 ohm-cm @Temperature 20.0 °C |
0.00000350 ohm-cm @Temperature 68.0 °F |
|
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |