Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Electrical Resistivity | 0.00000344 - 0.00000410 ohm-cm | 0.00000344 - 0.00000410 ohm-cm | Calculated from 42-50 %IACS |
Cadi 10WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Electrical Resistivity | 0.00000344 - 0.00000410 ohm-cm | 0.00000344 - 0.00000410 ohm-cm | Calculated from 42-50 %IACS |
Cadi 5TC Tungsten Carbide Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |