Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000331 - 0.00000391 ohm-cm | 0.00000331 - 0.00000391 ohm-cm | Calculated from 44-52 %IACS |
Cadi 15WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Electrical Resistivity | 0.00000331 - 0.00000366 ohm-cm | 0.00000331 - 0.00000366 ohm-cm | Calculated from 47-52 %IACS |
Cadi 5WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |