Polymer Property : Electrical Resistivity = 0.00000283 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, 1/2 Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, 1/4 Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, Annealed
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, Extra Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Eagle Brass 18665 MSP1, Spring
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..