Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000257 ohm-cm | 0.00000257 ohm-cm | (67% IACS) |
CMW® D50 Silver Nickel Contact Material ASTM B693 For electrical contacts; resistant to mechanical wear.Information provided by CMW Inc. |