Polymer Property : Electrical Resistivity = 0.00000236 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000236 ohm-cm
0.00000236 ohm-cm
(73% IACS)
CMW® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
For electrical contacts; resistant to welding and high surge currents.Information provided by CMW Inc.