Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000190 ohm-cm | 0.00000190 ohm-cm | |
PSM Industries Pacific Sintered Metals Copper CU-143-W Powdered Metal High electrical and thermal conductivity, Good for heat sinks and electrical problemsInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Electrical Resistivity | 0.00000190 - 0.00000200 ohm-cm | 0.00000190 - 0.00000200 ohm-cm | |
Williams Advanced Alloys C106 Solder Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i.. |
|||
Electrical Resistivity | 0.00000190 ohm-cm | 0.00000190 ohm-cm | 92 % IACS |
CMW® ELKONITE 2110 sintered tungsten-silver wire ELKONITE® 2110 is a sintered tungsten-silver material that is made into wire. This wire can be cold headed into rivet contacts or discs, which can be brazed, to rivets or other backings. ELKONITE®.. |
|||
Electrical Resistivity | 0.00000190 ohm-cm | 0.00000190 ohm-cm | 90 % IACS |
CMW® ELKONIUM 73 Copper Cadmium Alloy with Au/Ag-Cladding ELKONIUM 73 alloy is a silver, copper, cadmium and gold material marketed by CMW with high electrical and thermal properties. It is designed as an economical rivet type contact for AC applications r.. |