Electrical Properties Metric English Comments
High Voltage Arc Resistance to Ignition (HVAR) 120 - 180 sec

@Thickness 3.00 mm
120 - 180 sec

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..