Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow
Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 0.550 mm
15 - 30 arcs

@Thickness 0.0217 in
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
High Amp Arc Ignition, HAI 15 - 30 arcs

@Thickness 1.50 mm
15 - 30 arcs

@Thickness 0.0591 in
BK
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..