Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 35 sec @Thickness 0.711 mm |
35 sec @Thickness 0.0280 in |
UL 746A |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |