Polymer Property : Melt Temperature = 999 °C
Polymer Property :
Melt Temperature =
999 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Melt Temperature
999
-
1060
°C
1830
-
1940
°F
Wieland Eco E4 Casting Alloy
Silver-palladium casting alloyApplications: crowns, short span bridges, long span bridgesDental