Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | >= 214 °C | >= 417 °F | |
Voloknohim PA 6-120/321 Nylon 6 For production of plastics and industrial goods used in machine building and motor industry. Nylon 6 bright, not dyed and (or) heat stabilizedInformation provided by Voloknokhim |