Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 40.0 - 110 °C | 104 - 230 °F | Average value: 76.5 °C Grade Count:5 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |