Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 375 °C | 707 °F | |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |