Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable JA306BA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJK501L Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC304 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC302LR Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 166 °C | 320 - 331 °F | |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 166 °C | 320 - 331 °F | |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 166 °C | 320 - 331 °F | |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |