Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 256 °C | 493 °F | LCL-PR29 |
Intercontinental Polymers HoPET 721 HoPET Polymer Type - Clear, Polyester Pellets Applications: Engineering ResinInformation provided by Intercontinental Polymers. |