Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 199 - 201 °C | 390 - 393 °F | |
Tempia Polylactic acid (PLA) Resin A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thicknes.. |