Polymer Property : Melt Temperature = 1940 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 1060 - 1180 °C
1940 - 2160 °F
Wieland Porta AB 76 Casting Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, ceramic veneering, acrylic veneeringDental
Melt Temperature 1060 - 1140 °C
1940 - 2090 °F
Wieland Porta Geo Ti PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental