Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1015 - 1055 °C | 1859 - 1931 °F | |
Wieland Porta IP V-1 Solder Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental |
|||
Melt Temperature | 1015 - 1030 °C | 1859 - 1886 °F | |
Wieland Porta IP V-2 Solder Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental |