Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 938 - 1080 °C | 1720 - 1980 °F | |
Wieland Porta Aurium PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Melt Temperature | 938 - 999 °C | 1720 - 1830 °F | |
Wieland Portagold Casting Alloy Gold casting alloyApplications: inlays/onlays, crownsDental |