Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 921 - 1040 °C | 1690 - 1900 °F | |
Wieland Porta Optimum PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |