Polymer Property : Melt Temperature = 1110 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 1040 - 1110 °C
1900 - 2030 °F
Wieland BioPorta G PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Melt Temperature 1050 - 1110 °C
1920 - 2030 °F
Wieland Porta Aurium 2 PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Melt Temperature 1020 - 1110 °C
1870 - 2030 °F
Wieland Porta Maximum NF PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..