Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 971 - 1070 °C | 1780 - 1960 °F | |
Wieland BioPortadur Casting Alloy Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |