Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 90.0 min @Temperature 25.0 °C |
90.0 min @Temperature 77.0 °F |
|
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |