Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 240 - 360 min @Temperature 25.0 °C |
240 - 360 min @Temperature 77.0 °F |
|
Parker Chomerics CHO-BOND 592 Conductive Epoxy Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical condu.. |