Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 4.00 Month @Temperature 4.00 °C |
4.00 Month @Temperature 39.2 °F |
|
Hexcel® HexPly® 8551-7 Epoxy Matrix, Carbon Tape Form Information provided by HexCel |