Polymer Property : Gel Time = 80.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 80.0 - 120 min

@Temperature 150 °C
80.0 - 120 min

@Temperature 302 °F
Hexcel® HexPly® M39-X7B Epoxy Matrix
HexPly® M39-X7B is specifically designed for prepreg applications with unidirectional fibers and short curing cycles for sporting (e.g. racket production) and industrial applications. HexPly® M39-..