Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 7.00 min | 7.00 min | |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 3K PW Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Gel Time | 7.00 min | 7.00 min | |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |