Polymer Property : Gel Time = 62.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 62.0 min
62.0 min
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin
3M Scotchcast Re-enterable Electrical Resin 2123 is a soft, two-part polybutadine resin encapsulant designed especially for re-enterable splice protection. It is formulated for virtually every elect..