Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 40.0 - 50.0 min @Temperature 25.0 °C |
40.0 - 50.0 min @Temperature 77.0 °F |
100 gram mass |
Lord Adhesives Thermosetâ„¢ UR-340 Two Component Urethane Encapsulant Lord UR-340 is a two component, room temperature curing, urethane encapsulating compound. It is low in viscosity and has excellent flow characteristics. Its flexibility, low modulus characteristics,.. |