Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 180 - 300 min @Temperature 25.0 °C |
180 - 300 min @Temperature 77.0 °F |
Thin Film |
Trelleborg Emerson & Cuming EP551 Adhesive Clear unfilled adhesive for use with complete range.All information provided by Trelleborg Emerson & Cuming |
|||
Gel Time | 180 - 300 min @Temperature 25.0 °C |
180 - 300 min @Temperature 77.0 °F |
Thin Film |
Trelleborg Emerson & Cuming EP692 Sealer Sealer compatible with complete rangeAll information provided by Trelleborg Emerson & Cuming |