Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 8.00 - 16.0 min @Temperature 177 °C |
8.00 - 16.0 min @Temperature 351 °F |
|
Hexcel® HexPly® 8551-7 Epoxy Matrix HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPl.. |