Polymer Property : Gel Time = 15.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 15.0 min
15.0 min
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..
Gel Time 15.0 min
15.0 min
At 77°F using 1.25% #69 Catalyst
Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
Description:#77 Molding Resin is ideal for general purpose part fabrication and for building low cost molds. An internal thickening agent has been added to prevent drainage on vertical surfaces, yet..
Gel Time 15.0 min
15.0 min
At 77°F using 1.25% #69 Catalyst
Fibre Glast 83 Waxed Polyester Laminating Resin
Description: #83 Waxed Polyester Laminating Resin is a prepromoted, thixotropic general purpose resin. #83 contains styrene wax for low styrene emissions and to prevent air inhibition. #83 is a waxe..
Gel Time 15.0 - 30.0 min

@Temperature 65.0 °C
15.0 - 30.0 min

@Temperature 149 °F
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant
Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All..
Gel Time 15.0 min

@Temperature 150 °C
15.0 min

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant
LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle..
Gel Time 15.0 min

@Temperature 25.0 °C
15.0 min

@Temperature 77.0 °F
Thin Film
Trelleborg Emerson & Cuming EP679 Patch Paste
Blue patch pasteAll information provided by Trelleborg Emerson & Cuming