Processing Properties Metric English Comments
Gel Time >= 1440 min
>= 1440 min
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..