Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 13.0 min @Temperature 177 °C |
13.0 min @Temperature 351 °F |
|
Hexcel® HexPly® 8552 Epoxy Matrix HexPly® 8552 is an amine cured, toughened epoxy resin system supplied with unidirectional or woven carbon or glass fibers. HexPly® 8552 is recommended for structural applications requiring high st.. |
|||
Gel Time | 13.0 min @Temperature 93.0 °C |
13.0 min @Temperature 199 °F |
10 g |
Abatron AboCast 8110-8/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |