Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.500 - 0.670 min | 0.500 - 0.670 min | |
Dow BETAFOAM™ 87100/87124 BETAFOAM™ 87100/87124 is a high-density, all-water blown rigid polyurethane foam. These components were engineered to produce a foam for increasing stiffness of body structure cavities. Foam is p.. |