Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Cooling | 15 sec | 15 sec | |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |