Processing Properties Metric English Comments
Cycle Time - Cooling 10.0 - 20.0 sec
10.0 - 20.0 sec
Average value: 15.0 sec Grade Count:18
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..