Processing Properties Metric English Comments
Clamp Pressure 26.7 - 62.3 MPa
3870 - 9040 psi
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..